Our Swimming Pool Waterproofing Membrane is a coating that is used to a thickness of over 2000 microns. The two reactants are combined, poured at first glance that must be covered and scattered utilizing froth rollers. Unique solids and Polyurethane Groundwork that is tolerant to clamminess, seals the surface of the solid before the main coat is used. The covering can be used in damp conditions. There is zero impact because of the provided Swimming Pool Waterproofing Membrane being submerged into water. According to Strategy 7.4 of ASTM D 570 the immersion pressure gain is under 0.60%.
Price range- 75-125rs. / sq.ft.
Area specified required - 7500sq.ft
Property | Test Standard | Result â Drythane | Result â Competitor |
---|---|---|---|
Solid Content (%) | ASTM D 2697 | 100% | 55-60% |
Solvent Content (%) | ASTM D 2697 | 0% | 40-45% |
Adhesion To Concrete | ASTM D 4541 | > 300 Psi (2.0 N/mm2) | 65 Psi (0.45 N/mm2) |
Tensile Strength | ASTM D 412 | 2,908 Psi (20 N/mm2) | 14.50 Psi (0.10 N/mm2) |
Elongation @ Break | ASTM D 412 | > 50% | > 500% |
Hardness (Shore D) | ASTM D 2240 | 64.2 | 08 |
Water Absorption | ASTM D 570 | 0.59% | > 5% |
Chemical Resistance | ASTM D 570 | 10% H2SO4 = 0.26% | Sample Destroyed |
Water Vapour Transmission | ASTM E 96 | 1.85 gms/M2/day (Average) | > 5 gms/M2/Day |
Flexibility | ASTM D 522 | 1.50 mm film passes 12 mm mandrel | 1.50 mm film passes 12 mm mandrel |
Abrasion Resistance | ASTM D 4060 | 100 mgs (Weight Loss) | Not tested but visibly very poor |